Page 27 - tmp
P. 27
membrane, paint or other sealer. If you suspect that the This product has a maximum shelf life of one year when stored
concrete has been previously sealed, call Polycoat Products off the ground in a dry area at 50º to 110ºF, in the original
technical support for further instructions. sealed container.
CHECK FOR MOISTURE Clean-Up
Concrete must be dry before application of this floor coating Clean-up mixing station, tools and application equipment
material. Concrete moisture testing must occur. Calcium immediately after completion. Use suitable solvent as
chloride testing or “In-situ” relative humidity testing is specified by Polycoat Products’ Technical Services Team or
recommended. Test methods can be purchased at www.astm. if permissible by law, xylene, as a general over-the-counter
org, see ASTM F1869-11 or F2170-11, respectively or follow solvent. Observe all fire hazards, legal, and health and safety
manufacturer’s instructions. Readings must be below the precautions when handling or storing solvents, particularly
defined threshold as specified for each Polycoat Products in confined spaces. Make sure the working area is well
system to be installed directly to the concrete substrate. ventilated at all times during application and curing times.
Please refer to the appropriate Technical Data Sheet for this Dispose all excess materials, packaging, and other waste in
information. accordance with federal, state, and local regulations.
CHECK THE TEMPERATURE & HUMIDITY Maintenance
Floor temperature and materials should be between 65°F Occasionally inspect the installed floor by spot cleaning and
(18°C) and 90°F (32°C). Humidity must be less than 95%. DO spot repairing any damaged or cracked areas. To prolong
NOT coat unless floor temperature is more than (5ºF) over the life of the flooring system, a daily cleaning maintenance
the dew point.
program is highly recommended to ensure the floor is safe
SURFACED PREPARATION for its intended purpose.
Requires ICRI CSP 3 First Aid
This product requires proper surface profile to perform as Warning! Eye and skin irritant. May cause dermatitis and
expected. Substrate must be mechanically profiled (ASTM sensitization. In case of contact: Avoid contact with eyes, skin
4259-83), clean, sound, and dry. or clothing. Avoid breathing vapor, mist or spray. Use with
Mixing good ventilation.
The temperature of the (A) and (B) portions should be between Eyes: Immediately flush with water for at least 15 minutes.
70ºF and 80ºF (20º-25ºC). Mix them separately to ensure a Skin: Immediately remove from skin with dry cloth followed
uniform consistency. For a 3 gallon kit add (Side-B) into by thorough washing with soap and water.
(Side-A) in a 3.5 gallon bucket. Mix contents thoroughly until Inhalation: Remove to fresh air. If breathing is difficult, give
all components are completely incorporated and no streaking oxygen.
is observed. Thinning is not recommended. The portions of
each side is accurately measured to ensure optimum product Ingestion: Immediately call a Poison Center/Doctor. Do NOT
performance. Pouring from one container to the other (boxing) induce vomiting. If vomiting occurs naturally, lie on your side,
during mixing is very helpful in ensuring complete mixing. in the recovery position.
Mix for 2 minutes. Limitations
Application This product is best suited for application in temperatures
APPLICATION EQUIPMENT between 60°F and 90°F. Do not use to grout coat over
Tools: 3” Disposable brush, low speed drill (450 rpm) with a aggregate. [Certain colors appear white when scratched such
3.5” Jiffler blade, 3/8” nap non-shedding phenolic core roller, as blue based.] Higher temperatures will result in faster dry
and flat rubber squeegee. times and/or poor workability. Color may vary due to batch-
to-batch variation, especially in higher temperature. Do not
ROLL ON apply over ponding water. Always read and understand the
After mixing all contents as instructed, immediately pour specific product data guide and SDS sheets before using this
out into a ribbon on the surface. Squeegee the material out product. For more information contact Polycoat Products.
evenly and check for desired film thickness by using a wet-film USE PRODUCT AS DIRECTED. KEEP OUT OF THE REACH OF
thickness gauge. Back-rolling and then cross rolling is critical. CHILDREN.
Allow to dry minimum of 12 hours before recoat.
Storage
Limited Warranty: Please read all information in the General Guidelines, Technical Data Sheets, Guide Specifications and Safety Data Sheets (SDS) before applying material. These products are for professional use only
and preferably applied by professionals who have prior experience with the Polycoat Products materials or have undergone training in application of Polycoat Products materials. Published technical data and instructions are
subject to change without notice. Contact your local Polycoat Products representative or visit our website for current technical data, instructions, and project specific recommendations.
Polycoat Products warrants its products to be free of manufacturing defects and that they will meet Polycoat Products’ current published physical properties. Seller’s and manufacturer’s sole responsibility shall be to
replace that portion of the product which proves to be defective. There are no other warranties by Polycoat Products of any nature whatsoever expressed or implied, including any warranty of merchantability or fitness for
a particular purpose in connection with this product. Polycoat Products shall not be liable for damages of any sort, including remote or consequential damages resulting from any claimed breach of any warranty whether
expressed or implied. Polycoat Products shall not be responsible for use of this product in a manner to infringe on any patent held by others. In addition, no warranty or guarantee is being issued with respect to appearance,
color, fading, chalking, staining, shrinkage, peeling, normal wear and tear or improper application by the applicator. Damage caused by abuse, neglect and lack of proper maintenance, acts of nature and/or physical movement
of the substrate or structural defects are also excluded from the limited warranty. Polycoat Products reserves the right to conduct performance tests on any material claimed to be defective prior to any repairs by owner,
general contractor, or applicator.
Disclaimer: All guidelines, recommendations, statements, and technical data contained herein are based on information and tests we believe to be reliable and correct, but accuracy and completeness of said tests are not
guaranteed and are not to be construed as a warranty, either expressed or implied. It is the user’s responsibility to satisfy himself, by his own information and test, to determine suitability of the product for his own intended use,
application and job situation and user assumes all risk and liability resulting from his use of the product. We do not suggest or guarantee that any hazard listed herein are the only ones which may exist. Neither seller nor manufacturer
shall be liable to the buyer or any third person for any injury, loss or damage directly or indirectly resulting from use of, or inability to use, the product. Recommendations or statements, whether in writing or oral, other than those
contained herein shall not be binding upon the manufacturer, unless in writing and signed by a corporate officer of the manufacturer. Technical and application information is provided for the purpose of establishing a general profile
of the material and proper application procedures. Test performance results were obtained in a controlled environment and Polycoat Products makes no claim that these tests or any other tests accurately represent all environments.